+86 139 2552 1330 sales@cx-solenoid.com Dongguan, Guangdong, China
Engineering response within 2 working days
Technical

Solenoid Force vs. Stroke Explained

Why the force quoted on a datasheet is not the force you get. How the force-stroke curve is measured, and how to read it for a real mechanism.

Updated 2026-11-23 · 9 min read · Written and reviewed by the Cixin engineering team, Dongguan

Double-latching solenoid used to illustrate the force-stroke relationship
A double-latching part. Its hold force behaves like the open-gap curve below: strongest when closed.

Force is a curve, not a number

If you remember one thing about solenoid force, make it this: the number on the front page of a datasheet is the best number the part can produce, and it is probably not the number your mechanism will see. Solenoid force peaks when the air gap is fully closed, which is the moment the plunger has finished its travel and no longer needs the force. What you actually need is force at the start of motion and along the way, and those are the numbers that shrink.

This trips up experienced engineers too, not just buyers. A datasheet that says "50 N" is technically honest and practically useless until you know the stroke condition attached to it.

Why the curve falls so fast

The physics is not mysterious. Magnetic force across an air gap scales roughly with the inverse square of the gap length. Double the gap and you get about a quarter of the force. That inverse-square behaviour is why the force-stroke curve looks like a cliff: gentle and strong near the closed position, then falling away steeply as the plunger pulls back.

Here is a typical measured curve for a 25 mm tubular frame running at 24 V DC and 18 W:

Read the chart the way your mechanism will live on it. At 1 mm of remaining travel the part still delivers 78 N. At 10 mm, the full stroke, it delivers 9 N. If your load needs 30 N to start moving, this part cannot do the job at full stroke no matter what the front page of the datasheet promises. You would need a bigger frame, a shorter stroke, or a mechanism that presents a lighter load early in the travel and a heavier one late.

How to read a datasheet force figure properly

Three conditions sit behind every published force number, and all three deserve a question.

At what stroke? If the datasheet shows a curve, find your stroke on the x-axis and read down. If it shows only one number, assume it was taken near the closed gap unless someone confirms otherwise in writing.

At what temperature? Coil resistance rises with temperature. A coil measured cold at 25 °C delivers noticeably more force than the same coil after an hour of cycling, when the winding sits at 80 or 90 °C. The hot-force penalty is typically 10 to 20 percent, sometimes more. If your application cycles continuously, you must design to hot force, and that means asking the supplier for the hot figure.

At what voltage? Force scales with the square of ampere-turns, so a 20 percent voltage droop costs you around 36 percent of force. Battery-powered products live on drooping supplies. A lock specified at a fresh 12.6 V will feel weak at 10.5 V, which is exactly the voltage where the customer decides whether the product works.

Heat derates the curve, quietly

The hot-force effect deserves its own paragraph because it hides. In bench testing everyone measures cold, at a bench supply, with the part sitting in open air. In the product, the same coil sits inside a housing, cycling against a duty spec, in an enclosure that traps heat. All three differences push in the same direction, and they compound.

The practical habit that catches this: after any thermal test, re-measure force immediately, while the part is still hot. The number you get will be lower than the datasheet, and that lower number is the real one. If the margin between hot force and your load is thin, the design is not finished.

Design tricks that buy back force

When the curve and the load curve do not fit, you have more options than just picking a bigger part.

Shorten the working stroke. Even 2 mm saved moves you far up the curve, because of the inverse-square behaviour. A cam or lever that turns 6 mm of solenoid travel into 6 mm of bolt travel with a better force profile often beats a bigger solenoid on cost, weight and noise all at once.

Load the stroke late. Springs that are soft early and stiff late match the solenoid curve better than constant-rate springs. Progressive-rate springs exist for exactly this reason.

Use a cone-faced plunger. Conical plunger faces trade peak force near the closed gap for a flatter curve across the stroke. If your load is roughly constant through the travel, a cone face can outperform a flat face that is stronger only where you do not need it.

Check the supply, not just the coil. A capacitor across the coil or a brief over-voltage pulse at engagement can recover starting force on battery products without raising steady-state heat. This is standard practice in lock design and it costs cents.

Put your load curve on the part's curve

The whole discipline reduces to one drawing: the mechanism's force requirement plotted against stroke, with the solenoid's force-stroke curve laid over it. If the solenoid curve sits above the load curve everywhere, with margin, the design works. If the lines cross anywhere, the mechanism will stall at that point, no matter how impressive either number looked alone.

If you send us the load curve, even as three hand-measured points, we will return the closest catalogue part with its real curve overlaid, hot-force corrected. That exchange usually saves a prototype round. The engineering enquiry form takes exactly this kind of input, and the duty cycle guide explains the temperature side of the correction.

Frequently asked questions

Why is solenoid force highest when the gap is closed?

Magnetic force across an air gap scales with the inverse square of gap length. At a closed gap the reluctance of the magnetic circuit is minimal, so flux density peaks, and force peaks with it. This is why datasheet numbers quoted without a stroke condition are usually closed-gap figures.

How much force does a solenoid lose when hot?

Typically 10 to 20 percent between a cold coil at 25 °C and the same coil at its normal operating temperature, because copper resistance rises and current falls at constant voltage. Continuous-duty applications must be sized on the hot figure.

What happens if the voltage drops below rated?

Force falls with the square of the voltage-to-rated ratio. A 20 percent droop costs about 36 percent of force. Battery products should be specified at the minimum battery voltage under load, not at full charge.

Does a bigger coil always mean more force?

More ampere-turns mean more force, but a bigger coil in the same frame may just add heat. Force density depends on the whole magnetic circuit: frame cross-section, plunger material and gap geometry. Ask for force at your stroke and duty, not coil size.

Related reading

Have a drawing, a sample, or just a stroke and a force?

Send it over. An engineer reviews every enquiry and replies with a feasible concept, not a brochure.